50% Composite A (LF) Dispersion

General Description

Aqueous dispersion containing a proprietary blend of sulphur, accelerators and antioxidant which is used in latex foam manufacture using NR latex, in conjunction with Aquaspersions' 50% Composite B (LF) Dispersion.

Product Features

Supplied as a stable aqueous dispersion

Proven in NR latex foam manufacture with typical dosage of 2.2phr (dry/dry basis) based upon 10-12 hours' maturation, curing temperature of 105 deg.C and curing time of 1.5 hours

Compatible with NR latex

Cost effective

To enquire about this product, please fill out the details below:

Typical Properties

Total Solid Content

52.00%

Active Solid Content

50.00%

Viscosity (RV,sp4@20rpm)

850cps

Specific Gravity

1.20g/cm3

pH

9.00

Particle Size (um) D95N

<5.00um